Al2O3 is a widely used support in preparing Fe2O3-based oxygen carriers (OCs) due to its low cost and adjustable texture. Yet various Fe2O3­-Al2O3 synthesized with different Al2O3 precursors (such as α-Al2O3, γ-Al2O3, β-Al2O3, and hydrate nitrate of Al, etc.) and preparation methods (mechanical mixing, sol-gel, impregnation, etc.) have been reported in multiple chemical looping process, correspondingly diverse performances were presented, whereas mechanisms of how Al2O3 influencing the performance of Fe2O3-based OCs are insufficient, which causes a confusion in choosing Al2O3. In the present work, five types of Al2O3 precursors were adopted to prepare the Fe2O3­-Al2O3 by mechanical mixing, then the reactivity and stability of these OCs were assessed in chemical looping hydrogen generation process in a fixed bed reactor. Results showed that pure Fe2O3 and Fe2O3-­inert Al2O3 have a low reactivity with CH4, while Fe2O3 supported by the Al2O3 from AlOOH, activated Al2O3 and Al(OH)3 present high reactivity achieving nearly 100% biomass gasified gases conversion. X-ray diffraction (XRD), scanning electronic microscope (SEM) and micro texture analysis on the calcined Al2O3 precursors and as-prepared OCs revealed that various crystalline phases possessed for the calcined Al2O3 precursors, and close relationship exists between these calcined Al2O3 precursors and Fe2O3-based OCs in micro photograph, BET surface area and pore volume. Despite the fact that α-Al2O3 supported Fe2O3-based OCs presented low CO2 selectivity and low H2 yield, these Fe2O3-based OCs with high BET surface area and pore volume, such as Fe2O3­-AlOOH and Fe2O3-activated Al2O3, produced high purity CO2 and high production of H2, and showed a stable behavior in cycling tests compared with other Fe2O3-based OCs. Finally, the mechanism of Al2O3 influencing the performance of Fe2O3-based OCs was discussed from the perspective of lattice oxygen diffusion and micro texture effects.
 
关键词
Al2O3; Methane; Chemical Looping; Hydrogen; Hercynite
报告人
高子翔
学生 东南大学

稿件作者
高子翔 东南大学
肖睿 东南大学
发表评论
验证码 看不清楚,更换一张
全部评论
重要日期
  • 会议日期

    04月06日

    2023

    04月08日

    2023

  • 04月04日 2023

    报告提交截止日期

  • 04月15日 2023

    注册截止日期

  • 04月30日 2023

    初稿截稿日期

主办单位
昆明理工大学
承办单位
昆明理工大学
联系方式
移动端
在手机上打开
小程序
打开微信小程序
客服
扫码或点此咨询