Molecular dynamics simulation of ceramic polyolefin for fire resistant cable
Fire resistant cable; Ceramic polyolefin; Molecular dynamics simulation; Material selection.
全文被拒
Changlong Yang / State Grid Shenyang Power Supply Company
Min Gong / Chongqing Taishan Cable Co. Ltd
Fan Yang / Chongqing university
Jiaming Liang / Chongqing university
Peng Jin / State Grid Liaoning Electric Power Co. Ltd
In order to study the mechanism of high temperature environment’s influence on the mechanical properties and interparticle interactions of ceramic polymer materials for fire-resistant cables, the equivalent models of three ceramic polyolefin formulations were established according to the distribution proportion of each material. With the assistance of molecular simulation software, molecular dynamics simulation was carried out from the microcosmic point of view. The results show that with the increase of temperature, the intermolecular interaction weakens, the bulk modulus decreases, the shear modulus decreases, and the fractional free volume increases. The formulation with the most significant intermolecular interaction at high temperature, the formulation with the largest mechanical modulus at the same temperature and the formulation with the slowest increase of fractional free volume with temperature’s increase is the mixture system of ceramic ethylene butene copolymer and 28% EVA. The simulation results can provide reference for the selection of polyolefin ceramic materials for fire resistant cables.

 
重要日期
  • 会议日期

    11月02日

    2020

    11月04日

    2020

  • 10月27日 2020

    初稿截稿日期

  • 11月03日 2020

    报告提交截止日期

  • 11月04日 2020

    注册截止日期

  • 11月17日 2020

    终稿截稿日期

主办单位
IEEE IAS Student Chapter of Huazhong University of Science and Technology (HUST)
承办单位
Huazhong University of Science and Technology
联系方式
移动端
在手机上打开
小程序
打开微信小程序
客服
扫码或点此咨询